Synthesis and characterization of electrically conductive silicone rubber — TiB2 composites

Aparna M Joshi, Anjali A Athawale

Article ID: 644
Vol 2, Issue 2, 2019

VIEWS - 668 (Abstract) 203 (PDF)

Abstract


In this paper, electrically conductive composites comprised of silicone rubber and titanium diboride (TiB2) were synthesized by conventional mixing methods. Fine particles of TiB2 (in micron size) and 10 parts per hundred parts of rubber (phr) proportion of carbon black (XC-72) were used to make the composites with HTV silicone rubber. The composites were cured at appropriate temperature and pressure and the effect on the electrical properties was studied. The resistance of the silicone rubber is ~ 1015Ω which decreases to 1–2 kΩ in case of composites with negligible effect of heat ageing. The hardness increases by ~ 35% simultaneous to the decrease of ~ 47% in the tensile strength. Morphological characterization indicates the homogeneous dispersion of the fillers in the composite.


Keywords


Silicone Rubber; Electrical Conductivity; Titanium Diboride; Composite

Full Text:

PDF


References


1. Kathirgamanathan P. Light-coloured conductive fillers for the production of charge dissipative polymers. Polymer 1993; 34(7): 1549–1550.

2. Norman RH. Conductive rubbers and plastic. London: Elsevier publishing Co. Ltd.; 1970. p. 169–170.

3. Bhattacharya SK (editor). Metal-filled polymers: Properties and applications. New York: Marcel Dekker, Inc.; 1986. p. 355.

4. Gwaily SE, Nasr GM, Badawy MM. Thermal and electrical properties of irradiated styrene butadiene rubber-Metal composites. Egyptian Journal of Solids 2001; 24(2): 193–205.

5. Rajatendu S, Mithun B, Bandopadhyay S, et al. A review on the mechanical and electrical properties of graphite and modified graphite reinforced polymer composites. Progress in Polymer Science 2011; 36(5): 638–670.

6. Pan Y, Yu Z, Ou Y, et al. A new process of fabricating electrically conducting nylon 6/graphite nanocomposites via intercalation polymerization. Journal of Polymer Science B: Polymer Physics. 2000; 38 (12): 1626–1633.

7. Jeong DY, Ryub J, Lima YS. et al. Piezoresistive TiB2/silicone rubber composites for circuit breakers. Sensors and Actuators A: Physical 2009; 149(2): 246–250.

8. Tantawy FE. The interrelation among network structures, molecular transport of solvent, and creep behaviors of TiB2 ceramic containing butyl rubber composites. Journal of applied Polymer Science 2005; 98(5): 2226–2235.

9. Smith LP. The language of rubber: An introduction to the specification and testing of elastomers. 1st ed. London: Butterworth-Heinemann Ltd.; 1993. p. 257.

10. Blythe AR. Electrical resistivity measurements of polymer materials. Polymer Testing 1984; 4(2-4): 195–209.

11. Tantawy FE. Influence of solvent transport on physico-chemical properties of crosslinked butyl rubber filled with TiC ceramic. Polymer Degradation and Stability 2001; 73(2): 289–299.

12. Sood DK, Mukherjee S, Katselis G, et al. Modification of high-temperature oxidation of titanium diboride films by implantation with tantalum and titanium ions. Surface and Coatings Technology 1998; 103-104: 304–31.




DOI: https://doi.org/10.24294/can.v2i2.644

Refbacks

  • There are currently no refbacks.


Copyright (c) 2019 Characterization and Application of Nanomaterials

Creative Commons License
This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License.

This site is licensed under a Creative Commons Attribution 4.0 International License.